|  | HTM - fibre An alternative to STM-fibre. Advantages: - Reproducable quality on level of STM-fibre
- Cost level similar to STM-fibre
- Has its own production line
Datasheet HTM-fibre | Item | Unit | Standard | 3 year average | | Titre | dtex | 2,1 +/- 0,30 | 2,1 | | Tenacity | cN / dtex | ≥ 10,80 | 12,3 | | Young's Mod. | cN / dtex | ≥ 230 | 284 | | Extent. at Break | % | 6,5 +/- 2,5 | 7,10 | | Cut Length | mm | 5 or 6 | 5 or 6 | | Dispersability | 6 classes | 1 - 3 | 1 - 3 | | Moisture Regain | % | 5,0 | 5,0 | | Hot Water Solub. | % | ≤ 2,5 | 1,0 | | PDSC init. temp. | °C | ≥ 100 | 110 | | PDSC peak temp. | °C | ≥ 103 | 115 | | Sizing Agent | % | ≤ 0,70 | 0,05 | | Specific Gravity | | 1,29 | 1,29 |
|  |  |  | Bale-Packing of HTM-fibre |  | |
|
 |
|  |  |  |  Hegeler & Söhne GmbH & Co. KG
|